So far I've had pretty mixed results with paint finishes on the mangesiun KTM engine cases (mostly poor results with the paint peeling/rubbing off) and wondering if anyone has used an aquablast/polish & clear varnish finish to their cases and what was the long-term result?



VMX1963
//www.motorbikearchives.com

Tony Price

I bead blast my cases and use a self etching primer before I paint.  I also use thin coats and lightly wet sand between coats.

John D. says I over do it though, lol.


Tony
Tony

Larry Perkins

I have not had any peeling probs with the PJ1 paint.  It rubs off like stock in foot wear areas eventually but not peeling.

Larry P

OUCWBOY

I think it's all in how well you prep them before you pait.